Heze Great Bridge Chemical Co., Ltd.

Chlorobutyl Rubber CIIR139

Chlorobutyl Rubber CIIR139

Appearance: light yellow; weight of a bale — 30 ± 1 kg
Chlorine, wt %, within:1,10-1,40
Ash, wt %, max:0,50
Loss on drying, wt %, max:0,70
Send Inquiry
Description
Technical Parameters

introduce

A product obtained by chlorination of butyl rubber with unsaturation 1.8 mol% minimum

Appearance: light yellow; weight of a bale - 30 ± 1 kg

Package: EVA film; plastic container or metal container of type MB-5 (or its analogs)

Shelf life: 2 (two) years from the date of manufacture

Storage conditions:at the temperature not higher than 30 °C, in place protected from direct sunlight, atmospheric precipitation and pollution

Parameters

CIIR-139

Test method

Mooney viscosity ML 1+8 (125 °C), UM, within

33-44

para. 4.2 of TU or ASTM D 1646

Viscosity spread in a lot Mooney, MU, max

4

para. 4.2 of TU

Chlorine, wt %, within

1,10-1,40

para. 4.3 of TU or ASTM D 3566

Ash, wt %, max

0,50

para.4.4 of ТU or ISO 247 or ASTM D 5667

Non-staining antioxidant, wt %, min

0,05

para. 4.6 of TU

Loss on drying, wt %, max

0,70

para.4.7 of ТU or ISO 248 or ASTM D 5668

Curing characteristics, within:

- minimum torque МL, dNm

2,0-3,5

para. 4.9 of TU

- maximum torque, МH, dNm

6,5-10,0

para. 4.9 of TU

- time to cure start, tS1, minutes

0,8-2,2

para. 4.9 of TU

- time to 50% cure, t'(50) minutes

2,5-5,0

para. 4.9 of TU

- time to 90% cure, t'(90) minutes

6,5-11,0

para. 4.9 of TU

 

Hot Tags: chlorobutyl rubber ciir139, China chlorobutyl rubber ciir139 manufacturers, suppliers, factory